Specification of Different types of Pulp
Characteristics BCTMP Hardwood Softwood
Brightness (OSR) ISO 80 to 85 90 (±1) 90 (±1)
Breaking Length (Meter) 2500 ± 200 5000 10000
Burst Factor 20 (±5) 30 80
TEAR Factor 75 Minimum 75 100
Strength Index - N.R. 37.5 267
CSF SR 302/40 302/40 302/40
(Canadian Specification SR at 40° beating)
Calculation of Strength Index = (Burst Factor X Tear Factor X Breaking Length) / 302